Experiment no | Infill pattern | Nozzle temperature (°C) | Print speed (mm/sec) | Layer height (mm) | Infill density (%) |
---|---|---|---|---|---|
1 | Lines | 200 | 30 | 0.1 | 20 |
2 | Lines | 205 | 70 | 0.2 | 40 |
3 | Lines | 210 | 110 | 0.3 | 60 |
4 | Lines | 215 | 150 | 0.4 | 80 |
5 | Triangles | 200 | 70 | 0.3 | 80 |
6 | Triangles | 205 | 30 | 0.4 | 60 |
7 | Triangles | 210 | 150 | 0.1 | 40 |
8 | Triangles | 215 | 110 | 0.2 | 20 |
9 | Cubic | 200 | 110 | 0.4 | 40 |
10 | Cubic | 205 | 150 | 0.3 | 20 |
11 | Cubic | 210 | 30 | 0.2 | 80 |
12 | Cubic | 215 | 70 | 0.1 | 60 |
13 | Octet | 200 | 150 | 0.2 | 60 |
14 | Octet | 205 | 110 | 0.1 | 80 |
15 | Octet | 210 | 70 | 0.4 | 20 |
16 | Octet | 215 | 30 | 0.3 | 40 |