Table 2 Typical mix proportion for PC

From: Effect of aggregate gradation on the mechanical strengths and permeability properties of porous concrete

Ingredients

Quantity

Cementitious material

400 kg/m3

Water/cementitious material ratio

0.35

Coarse aggregate

1400 kg/m3

Water content

140 kg/m3