From: Wear behaviour of hybrid (boron carbide-graphite) aluminium matrix composites under high temperature
Sample designations | Composition | Al2618, Wt. % | Boron carbide (B4C), Wt.% | Graphite (Gr), Wt.% |
---|---|---|---|---|
S | Al 2618 | 100 | 0 | 0 |
S1 | Al 2618 + 3% B4C–2% Gr | 95 | 3 | 2 |
S2 | Al 2618 + 6% B4C–4% Gr | 90 | 6 | 4 |
S3 | Al 2618 + 9% B4C–6% Gr | 85 | 9 | 6 |
S4 | Al 2618 + 12% B4C–8% Gr | 80 | 12 | 8 |
S5 | Al 2618 + 15% B4C–10% Gr | 75 | 15 | 10 |