Parameter | Value |
---|---|
Stirring speed | 500 rpm |
Melting temperature | 750 °C |
Temp of melt during mixing | 630 °C |
Pouring temperature | 680 °C |
Wetting agent | Mg |
Grain size of SiC particles | 40–50 µm |
Grain size of TiB2 | 10–15 µm |
SiC preheating temperature | 200 °C |
TiB2 preheating temperature | 200 °C |
Position of stirrer in the melt | 1/3 of melt height from bottom |
Stirrer design | Four blade flat surface |
Stirring time | 10 min |
Mould preheating temp | 200 °C |
Gas flow rate | 2 lpm |