Test | Average test results | |
---|---|---|
Moslawi marble | Footing stone | |
Dry density, kN/m3 | 22.26 | 21.08 |
Compressive strength (dry condition), MPa | 14.36 | 9.36 |
Compressive strength (wet condition), MPa | 12.53 | 8.03 |
Modulus of rupture (dry condition), MPa | 8.24 | 2.55 |
Modulus of rupture (wet condition), MPa | 6.19 | 1.02 |
Total absorption, % | 0.21 | 8.40 |
Corrosion, % | 1.10 | 2.18 |