Group 1 Specimen

Compressive strength 7 days (N/mm2)

Compressive strength 28 days (N/mm2)

Slump (mm)

B1-0

26.5

35

90

B1-1

24.2

33.2

100

B1-2

20.5

30

115

B1-4

21.7

29.3

140

B2-0

26.7

35

90

B2-2

20.8

32

110

B2-4

22

30

145