From: Parameter optimization in the enhancement of MRR of titanium alloy using newer mixing method in PMEDM process
MRR in (g/min) at
% rise in MRR
No powder
2Â g/l of powder conc
Pre-mixing and pumping type PMEDM
0.033967
0.041586
22.43
Eductor-based PMEDM
0.042005
0.057856
37.74