Fig. 6From: Optimization of PC micro-drilling using a continuous CO2 laser: an experimental and theoretical comparative studyThe shape and diameter variation of the holes at the top surface when irradiated with laser powers of 2, 3, and 4 W at different exposure times (0.1, 0.15, and 0.2s) and different FPPs (−4 and 0mm)Back to article page