Table 4 Decomposition stages and percentage of weight loss for various compositions of polymer electrolytes (PMMA-LiTf-nanochitosan)

From: Thermal and mechanical studies of nanochitosan incorporated polymethyl methacrylate-based composite electrolytes

Samples

First decomposition temperature, °C

Second decomposition temperature, °C

Total weight loss, (%)

TF-NC0

118.5

322.2

86.1

TF-NC5

122.8

334.5

82.4

TF-NC10

126.7

335.3

74.9

TF-NC15

127.5

339.3

76.5

TF-NC20

130.2

342.94

69.1