Skip to main content

Table 8 The variation in electrochemical results of the reinforcing steel after exposure to accelerated corrosion setup

From: Enhancing corrosion resistance of RC pipes using geopolymer mixes when subjected to aggressive environment

Pipes indent.

E(i = 0) (mv)

i corrosion (μA/cm2)

Rp (kΩ.cm2)

Corrosion (μm/Y)

OPCA100 (MS-CL)

− 530.8

8.021

3.29

93.82

GPCB100 (MS-CL)

− 744.6

17.19 × 10−3

22.8

200.9 × 10−3

GPCC100 (MS-CL)

− 766.7

1.6973 × 10−3

1.28 × 103

19.85 × 10−3