Skip to main content

Table 3 Mix properties of geopolymer concrete

From: Studying the behavior of geopolymer concretes under repeated loadings

Metakaolin (MK) (kg/m3)

Sand (kg/m3)

Gravel (kg/m3)

Alkaline solution (lit/m3)

Water (lit/m3)

SP % (from metakaolin volume)

400

720

1100

180

40

3